Filament Settings and Drying

Starting points from the makers’ own guides. The label on your spool comes first.

Material

Drying PLA

50 °C, 6–8 h

122 °F

Dry it only once it shows the signs of wet filament. Until then a sealed bag with desiccant is enough.

Softens at about 60 °C, so it isn't for parts left in a hot car or in the sun.

Sources (6)
Compare PLA prices

Settings to start from

Nozzle
210 °C (410 °F)Range 200–220 °C
Bed
60 °C (140 °F)Range 55–65 °C
On Bambu's Cool Plate (also called the PLA Plate), 35 to 45 °C.
Part Fan
Full
Enclosure
No

Drying Chart

Temperatures in °C, with °F under each. Tap a material for its full settings.

Drying temperature and time, and starting nozzle and bed temperatures, for each filament material
MaterialDry atNozzleBed
PLADryer: Only if wet50122 °Ffor 6–8 h210410 °F60140 °F
PLA+ and Tough PLADryer: Only if wet50122 °Ffor 6–8 h215419 °F60140 °F
Silk PLADryer: Only if wet50122 °Ffor 6–8 h215419 °F60140 °F
Matte PLADryer: Only if wet50122 °Ffor 6–8 h215419 °F60140 °F
PETGDryer: Before printing60140 °Ffor 6–8 h240464 °F80176 °F
PCTGDryer: Before printing60140 °Ffor 4–6 h260500 °F80176 °F
ABSDryer: Before printing80176 °Ffor 4–8 h255491 °F100212 °F
ASADryer: Before printing80176 °Ffor 4–8 h255491 °F100212 °F
TPU (95A and Softer)Dryer: Before printing65149 °Ffor 6–8 h230446 °F45113 °F
Nylon (PA)Dryer: While printing80176 °Ffor 8–12 h260500 °FVaries by brand
Nylon Carbon Fiber (PA-CF, PA12-CF)Dryer: While printing80176 °Ffor 8–12 h275527 °FVaries by brand
Polycarbonate (PC)Dryer: Before printing80176 °Ffor 5–8 h265509 °F105221 °F
PC Blends (PC-ABS, PC Blend)Dryer: Before printing85185 °Ffor 5–8 h270518 °F110230 °F
PLA Carbon or Glass FiberDryer: Only if wet55131 °Ffor 6–8 h220428 °F60140 °F
PETG Carbon or Glass FiberDryer: Before printing65149 °Ffor 6–8 h250482 °F80176 °F
PVADryer: While printing80176 °Ffor 8–12 h220428 °F60140 °F
BVOHDryer: While printing50122 °Ffor 4–6 h210410 °F60140 °F
HIPSDryer: Before printing60140 °Ffor 4–6 h240464 °F100212 °F
Polypropylene (PP)Dryer: Only if wet60140 °Ffor 4–6 h230446 °F70158 °F
PEEK-CFDryer: While printing130266 °Ffor 4 h380–440716–824 °F140–155284–311 °F
PEI (ULTEM)Dryer: While printing140284 °Ffor 8 h370–420698–788 °F150–155302–311 °F

How to Tell Filament Is Wet

  • The surface turns rough, dull, or pitted.
  • You hear popping or hissing at the nozzle.
  • It strings more than it did when new.
  • Layers come out weak or brittle.

Nylon, PVA, and BVOH take up water fastest, then TPU, PC, and PETG. Dry them in a filament dryer at or under the listed temperature. Hotter than that and the strands stick together.

How to Store It

Put each spool back in a sealed bag or box with desiccant once you’re done. Keep it at room temperature, out of the sun. Print nylon, PVA, and BVOH straight from a dry box or a dryer.

Where the Numbers Come From

Every figure is from Bambu Lab, Prusa Research, Polymaker, Fiberlogy, Sunlu, and Spectrum, checked on November 7, 2026. The starting point is where those makers agree, and the range is what most of them publish. Where they disagree too much, we say so instead of picking a number. With a new brand, print a temperature tower, and follow your spool’s label and the maker’s safety data sheet.