ERYONE ABS Fiberglass

  • ABS
  • 1.75 mm
  • 1 kg
$24.99for 1 kg

In stockPrice checked

ColorBlack
Shop atERYONE

We may earn a commission when you buy through these links (affiliate disclosure).

Price History

Black at ERYONE

ERYONE’s price hasn’t changed since our records began on October 30.

Description

Glass Fiber ABS

Eryone Glass Fiber ABS is a glass fiber reinforced ABS material that supports printing in

open environments. It features a balanced combination of strength, rigidity, and warping resistance, with a heat resistance temperature of up to 82°C. The printing speed can reach 150 mm/s, and it

has a matte, fine sand-smooth surface texture. It offers excellent mechanical properties, thermal

stability, and printing efficiency, making it suitable for 3D printing applications that require certain

levels of strength, rigidity, and heat resistance, such as tooling fixtures, manufacturing jigs, enclosures, and structural components. Note: The glass fiber content is 10%.

Part I: Suggests Printing Parameters

Parameter

Set up

Nozzle temperature

240-280 ℃

Bed temperature

80-100℃

Bed materia

glass, PEI, spring steel plate

Bottom printing temperature

/

Sealed printing

Sealing print quality is better, supporting open

printing

Printing speed

30-150mm/s

Drying conditions

60℃, 4h

Part II: Physical Properties of Materials

Property

Testing Method

Unit

Typical Value

Density(g/cm³ at 21.5 ° C)

ASTM D792 (ISO 1183, GB/T 1033)

g/cm³

1.1

Vicat Softening Temperature(° C)

ASTM D1525 (ISO 306 GB/T 1633)

℃

/

Heat distortion temperature(° C)

ASTM D648 1.8MPa 0.45MPa

℃

82

Glass transition temperature (° C)

DSC, 10 ° C/min

℃

104

Melt Index(g/10 min)

220 ° C, 10kg 240 ° C, 2.16 kg

g/10min

30

Part III: Mechanical Properties of Printed Samples

Property

Test conditions

Test standards

unit

Typical Value

Tensile strength X-Y

50mm/min

GB/T 1040.4

MPa

37.2

Elastic modulus X-Y

50mm/min

GB/T 1040.1-2006

MPa

1735.8

Elongation at break X-Y

50mm/min

GB/T 1040.4

%

2.0

Tensile strength X-Z

50mm/min

GB/T 1843

MPa

19.2±4

Elastic modulus X-Z

50mm/min

GB/T 1040.1-2006

MPa

1651.2

Elongation at break X-Z

50mm/min

GB/T 1040.4

%

1.6

Bending strength

2mm/min

GB/T 9341

MPa

57.9

Bending modulus

2mm/min

GB/T 9341

MPa

2487.4

Charpy Impact strenght

2.75J

GB/T 1843

kJ/m2

6.2

Note: All splines are printed under the following conditions: printing temperature=270 ° C, printing

speed=150mm/s, base plate 90° C, filling=100%, nozzle diameter=0.4mm

Specifications

Material
ABS
Diameter
1.75 mm
Density
1.1 g/cm3
Heat Resistance
82 °C
Nozzle Temperature
240 to 280 °C
Bed Temperature
80 to 100 °C
Print Speed
30 to 150 mm/s
Drying
60 °C for 4 h
Glass Transition Temperature
104 C
Glass Fiber Content
10%
Tensile Strength X-Y
37.2 MPa
Tensile Strength X-Z
19.2 MPa
Bending Strength
57.9 MPa
Charpy Impact Strength
6.2 kJ/m2