ERYONE PLA Silk High-Speed Quadruple
- PLA Silk
- 1.75 mm
- 1 kg
In stockPrice checked
We may earn a commission when you buy through these links (affiliate disclosure).
Price History
Cold Flame Night Attack (Dark Purple & Magenta & Pink & Sky Blue) at ERYONE
ERYONE’s price hasn’t changed since our records began on October 30.
Description
Hyper Speed Quadruple Silk PLA
The Eryone High-Speed Silk PLA is a material with a thoroughly improved
formulation, offering significantly enhanced printing speeds compared to standard silk
PLA, reaching up to 500 mm/s. Additionally, its tensile strength has been notably
increased, with the Z-axis tensile strength reaching 20 MPa. This high-speed silk PLA
material delivers a more lustrous finish, presenting a silk-like appearance. The
brightness can be controlled by adjusting the temperature and speed: higher
temperatures and slower printing speeds result in increased brightness.
Part I: Suggests Printing Parameters
Parameter
Set up
Nozzle temperature
190℃-220℃
Bed temperature
55-70℃
Bed material
glass, PEI, spring steel plate
Bottom printing temperature
190℃-220℃
Sealed printing
Open Printing/closed printing
Printing speed
30-500mm/s
Drying conditions
65℃-75℃,12H
Part II: Physical Properties of Materials
Property
Testing Method
Unit
Typical Value
Density(g/cm³ at 21.5 ° C)
ASTM D792 (ISO 1183, GB/T 1033)
g/cm³
1.32
Vicat Softening Temperature(° C)
ASTM D1525 (ISO 306 GB/T 1633)
℃
56
Heat distortion temperature(° C
ASTM D648 1.8MPa 0.45MPa
℃
50
Glass transition temperature (° C)
DSC, 10 ° C/min
℃
57
Melt Index(g/10 min)
220 ° C, 10kg 240 ° C, 2.16 kg
g/10min
20±1.5
Part III: Mechanical Properties of Printed Samples
Property
Test conditions
Test standards
unit
Typical Value
Tensile strength X-Y
50mm/min
GB/T 1040.4
MPa
62.7
Elastic modulus X-Y
50mm/min
GB/T 1040.1-2006
MPa
1932.1
Elongation at break X-Y
50mm/min
GB/T 1040.4
%
2.3
Tensile strength X-Z
50mm/min
GB/T 1843
MPa
19.1
Elastic modulus X-Z
50mm/min
GB/T 1040.1-2006
MPa
1873.5
Elongation at break X-Z
50mm/min
GB/T 1040.4
%
1.9
Bending strength
2mm/min
GB/T 9341
MPa
86.7
Bending modulus
2mm/min
GB/T 9341
MPa
2917.3
Charpy Impact strenght
2.75J
GB/T 1843
kJ/m2
3.8
Note: All splines are printed under the following conditions: printing temperature=215 ° C, printing speed=80mm/s, base plate 60 ° C, filling=100%, nozzle diameter=0.4mm
Disclaimers
The values given in this data table are for reference and comparison only. They
should not be used for design specifications or quality control. The actual value may
vary depending on the printing conditions. The final performance of printed
components depends not only on the material, but also on the component design, environmental conditions, printing conditions, and so on. Product specifications are
subject to change without prior notice.
Specifications
- Material
- PLA Silk
- Diameter
- 1.75 mm
- Weight
- 1 kg
- Nozzle Temperature
- 190 to 220 °C
- Bed Temperature
- 55 to 70 °C
- Print Speed
- 30 to 500 mm/s
- Drying
- 65 to 75 °C for 12 H
- Density
- 1.32 g/cm3
- Heat Resistance
- 50 °C at 1.8 MPa
- Vicat Softening Temperature
- 56 C
- Glass Transition Temperature
- 57 C
- Melt Index
- 20 g/10min (220 C, 10 kg)
- Tensile Strength X-Y
- 62.7 MPa
- Tensile Strength X-Z
- 19.1 MPa
- Tensile Strength Z-Axis
- 20 MPa
- Elastic Modulus X-Y
- 1932.1 MPa
- Elongation at Break X-Y
- 2.3 %
- Bending Strength
- 86.7 MPa
- Bending Modulus
- 2917.3 MPa
- Charpy Impact Strength
- 3.8 kJ/m2