Description
The Eryone Burnt Titanium PLA filament is a material that exhibits captivating color
changes under different lighting and angles, creating a unique technological atmosphere and
providing an exceptional visual and tactile experience. This material has excellent toughness, producing no bubbles or odors during the printing process, and is resistant to clogging or
warping, ensuring outstanding shaping results and a smoother printing experience. Additionally, its Z-axis tensile strength reaches 34 MPa, with excellent interlayer adhesion.
Part I:Suggests Printing Parameters
Parameter
Set up
Nozzle temperature
190-220 ℃
Bed temperature
55-70℃
Bed materia
glass, PEI, spring steel plate
Bottom printing temperature
190-220 ℃
Sealed printing
Supports open printing; better results with enclosure.
Printing speed
30-100mm/s
Drying conditions
65-75℃, 12h
Part II: Physical Properties of Materials
Property
Testing Method
Unit
Typical Value
Density(g/cm³ at 21.5 ° C)
ASTM D792 (ISO 1183, GB/T 1033)
g/cm³
1.23
Vicat Softening Temperature(° C)
ASTM D1525 (ISO 306 GB/T 1633)
℃
54
Heat distortion temperature(° C)
ASTM D648 1.8MPa 0.45MPa
℃
53
Glass transition temperature (° C)
DSC, 10 ° C/min
℃
62
Melt Index(g/10 min)
220 ° C, 10kg 240 ° C, 2.16 kg
g/10min
6
Part III: Mechanical Properties of Printed Samples
Property
Test conditions
Test standards
unit
Typical Value
Tensile strength X-Y
50mm/min
GB/T 1040.4
MPa
52.2
Elastic modulus X-Y
50mm/min
GB/T 1040.1-2006
MPa
1737.5
Elongation at break X-Y
50mm/min
GB/T 1040.4
%
2.1
Tensile strength X-Z
50mm/min
GB/T 1843
MPa
34.2
Elastic modulus X-Z
50mm/min
GB/T 1040.1-2006
MPa
1623.7
Elongation at break X-Z
50mm/min
GB/T 1040.4
%
1.9
Bending strength
2mm/min
GB/T 9341
MPa
82.4
Bending modulus
2mm/min
GB/T 9341
MPa
2861.7
Charpy Impact strenght
2.75J
GB/T 1843
kJ/m2
3.7
Note: All splines are printed under the following conditions: printing temperature=210 ° C, printing speed=80mm/s, base plate 60° C, filling=100%, nozzle diameter=0.4mm
Specifications
- Material
- PLA
- Diameter
- 1.75 mm
- Weight
- 1 kg
- Nozzle Temperature
- 190 to 220 °C
- Bed Temperature
- 55 to 70 °C
- Print Speed
- 30 to 100 mm/s
- Drying
- 65 to 75 °C for 12 h
- Density
- 1.23 g/cm3
- Strength
- 52.2 MPa, 34.2 MPa
- Vicat Softening Temperature
- 54 C
- Heat Distortion Temperature
- 53 C
- Glass Transition Temperature
- 62 C
- Bending Strength
- 82.4 MPa
- Charpy Impact Strength